摘要: |
采用宏观检测、机械性能测试、腐蚀产物分析等方法,研究了威远页岩气田某平台失效管段的腐蚀失效原因。结果 表明,水中SRB、CO2、Cl-是引发腐蚀的主要因素。 |
关键词: 页岩气 地面管线 腐蚀 |
DOI:10.3969/j.issn.1007-3426.2019.05.016 |
分类号: |
基金项目:中国石油天然气股份有限公司重大科技专项“西南油气田天然气上产300亿立方米关键技术研究与应用——四川盆地气田开发地面系统安全清洁高效运行关键技术研究与应用”(2016E-0610) |
|
Analysis on corrosion of ground pipeline in Weiyuan shale gas field |
Mao Ting1,2,3, Yang Hang4, Shi Lei1,2,3
|
1. Research Institute of Natural Gas Technology, PetroChina Southwest Oil & Gasfield Company, Chengdu, Sichuan, China;2. National Energy High-Sour Gas Reservoir Exploitation and R&D Center, Chengdu, Sichuan, China;3. High Sulfur Gas Exploitation Pilot Test Center, CNPC, Chengdu, Sichuan, China;4. PetroChina Southwest Oil & Gasfield Company, Chengdu, Sichuan, China
|
Abstract: |
Through the methods of macroscopic detection, mechanical performance test and corrosion products analysis etc, the reasons of failure pipeline within some platforms in Weiyuan shale gas field were studied. The results show that the main factors causing corrosion are sulfate-reducing bacteria existing in water, carbon dioxide and chloride ions. |
Key words: shale gas surface pipeline corrosion |